I've got some tin tetrachloride which was originally in an anhydrous state but has absorbed a fair amount of moisture. As a result the crystals have become sticky and clumped together resulting in hard impacted lumps.

How would I go about processing it to revive it to its original form as it was when it was sold?

Offline Hunter2

  • Sr. Member
  • *****
  • Posts: 2178
  • Mole Snacks: +166/-48
  • Gender: Male
  • Vena Lausa moris pax drux bis totis
Re: Dehydrating and reviving tin tetrachloride (stannic chloride)
« Reply #1 on: May 08, 2016, 08:51:15 AM »
If Sncl4 gets wet it willbe form SnO2. So there is no way back. The only thing could be do do a destillation in vaccum to get rid off the tinoxides.